Product Detail:
⇒Chemical Composition
Alloy | element | Cr | Fe | C | Mn | Si | Mo | Co | W | P | S |
Hastelloy N | Min | 6 | 0.04 | 8.0 | |||||||
Max | 8 | 5 | 0.08 | 1.0 | 1.0 | 10.0 | 0.2 | 0.5 | 0.015 | 0.02 |
⇒Mechanical Properties
Alloy Status |
Tensile strengthRm Min ksi |
Wield strengthR P 0. 2 Min ksi |
Elongationin2 in., Min% |
Hastelloy N | 495 | 285 | 27 |
⇒Physical Properties
Density lb/in.3 | Annealing Temperature C° | Electric Conductivity %IACS |
8.86 | 1300-1400 | 11.5 |
⇒Standard
⇒Standard
Hastelloy Alloy Strip, Sheet, and Plate:ASTM B575, ASTM B906
Hastelloy Alloy Seamless Pipe: ASME SB572 ASME SB435 ASTM SB622
Hastelloy Alloy Welded Pipe: ASTM-B619.B626
Hastelloy Alloy Bar:ASTM B574
⇒Characteristics of Hastelloy N
Excellent corrosion resistance to most corrosive media in both oxidation and reduction atmospheres.
Has excellent resistance to pitting corrosion, crevice corrosion, and stress cracking corrosion.