Product Detail:
⇒Chemical Composition
Alloy | Element | C | Mn | P | S | Si | Cr | Ni | N | Mo | Cu | Fe |
S30815 | Min | 24.0 | 6.0 | 0.24 | 3.0 | Bal. | ||||||
Max | 0.03 | 1.2 | 0.035 | 0.02 | 0.8 | 26.0 | 8.0 | 0.32 | 5.0 | 0.5 | Bal. |
⇒Mechanical Properties
Alloy Status | Tensile strength
Rm Min Mpa
|
Yield strength
R P 0. 2 Min Mpa
|
Elongation
in2 in., Min % |
Hardness(HB) | Hardness(HRB) |
Annealed | 795 | 550 | 15 | 310 | 32 |
⇒Physical Properties
Density g/cms | Annealing Temperature ℃ | Electric Conductivity %IACS |
7.8 | 950 ~1100℃ |
⇒Standard
ASTM A240/ASME SA-240 Standard Specification for Chromium and Chromium-Nickel Stainless Steel PlateSheet, and Strip for Pressure Vessels and for Genera lApplications
ASTM A276 Standard Specification for Stainless Steel Bars and Shapes
ASTM A182/ASME SA-182 Standard Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges,Forged FittingS, and Valves and Parts for High-Temperature Service
ASTM A312/ASMES A312 Standard Specification for Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes
⇒Characteristics of 2507-UNS S32750
1.It has high compressive strength and impact strength
2.Low coefficient of thermal expansion and high thermal conductivity
3.It has strong resistance to stress corrosion cracking
4.It has strong corrosion resistance